Thermal Properties Metric English Comments
Thermal Conductivity 61.0 W/m-K

@Temperature 85.0 °C
423 BTU-in/hr-ft²-°F

@Temperature 185 °F
Indium Corp. Indalloy® 201 Sn-Zn Solder Alloy
Recommended for soldering to aluminum. Use flux #3. Zn causes high drossing, short shelf life as solder paste.Information provided by the manufacturer, Indium Corporation.