Indium Corp. 1072 VOC-Free Wave Solder Flux Containing Rosin

Category Fluid
Manufacturer Indium Corporation of America
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. 1072 VOC-Free Wave Solder Flux Containing Rosin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Wave Solder Flux 1072 is a halide-free, VOC-free, rosin flux specifically developed for wave-soldering, surface mount, mixed technology and through-hole electronic assemblies. This unique formulation is a new advancement in flux chemistry, combining the benefits of rosin with the environmental friendliness of a water-base product.FeaturesExcellent Surface WettingEliminates CleaningExcellent SolderabilityVOC-Free formulationContains RosinPhysical PropertiesColor: AmberInformation provided by the manufacturer, Indium Corporation of America.
Physical Properties Metric English Comments
Specific Gravity 1.017 g/cc

@Temperature 25.0 °C
1.017 g/cc

@Temperature 77.0 °F
1.017 g/cc

@Temperature 15.5 °C
1.017 g/cc

@Temperature 59.9 °F
Solids Content 5.0 %
5.0 %
Electrical Properties Metric English Comments
Insulation Resistance 5.20e+9 ohm

@Time 346000 sec
5.20e+9 ohm

@Time 96.0 hour
Control; IPC B24
7.67e+9 ohm

@Time 86400 sec
7.67e+9 ohm

@Time 24.0 hour
Control; IPC B24
Chemical Properties Metric English Comments
Acid Value 25
25
Descriptive Properties Value Comments
Flash Point None