Electrical Properties Metric English Comments
Insulation Resistance 7.67e+9 ohm

@Time 86400 sec
7.67e+9 ohm

@Time 24.0 hour
Control; IPC B24
Indium Corp. 1072 VOC-Free Wave Solder Flux Containing Rosin
Wave Solder Flux 1072 is a halide-free, VOC-free, rosin flux specifically developed for wave-soldering, surface mount, mixed technology and through-hole electronic assemblies. This unique formulati..