Physical Properties Metric English Comments
Specific Gravity 1.017 g/cc

@Temperature 25.0 °C
1.017 g/cc

@Temperature 77.0 °F
Indium Corp. 1072 VOC-Free Wave Solder Flux Containing Rosin
Wave Solder Flux 1072 is a halide-free, VOC-free, rosin flux specifically developed for wave-soldering, surface mount, mixed technology and through-hole electronic assemblies. This unique formulati..
Specific Gravity 1.017 g/cc

@Temperature 15.5 °C
1.017 g/cc

@Temperature 59.9 °F
Indium Corp. 1072 VOC-Free Wave Solder Flux Containing Rosin
Wave Solder Flux 1072 is a halide-free, VOC-free, rosin flux specifically developed for wave-soldering, surface mount, mixed technology and through-hole electronic assemblies. This unique formulati..