I. Stern N1921 General Purpose Crystal Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Transparent Grade
Manufacturer I. Stern & Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF I. Stern N1921 General Purpose Crystal Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features:Excellent ProcessabilityEasy FlowApplicationsDisposable PackagingHousewaresCosmetics PackagingAgency RatingsFDA Title 21 CFR 177.1640UL File E220962Information provided by I. Stern & Co. Inc.
Physical Properties Metric English Comments
Melt Flow 20 g/10 min
20 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 37.0 MPa
5370 psi
ASTM D638
Elongation at Yield 1.3 %
1.3 %
ASTM D638
Flexural Strength 89.6 MPa
13000 psi
ASTM D790
Flexural Modulus 3.20 GPa
464 ksi
ASTM D790
Izod Impact, Notched 0.0801 J/cm
0.150 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 72.8 °C
163 °F
ISO
Vicat Softening Point 82.8 °C
181 °F
ISO
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in