Hyosung Topilene J301CP PP

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Hyosung Co.
Trade Name Topilene
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hyosung Topilene J301CP PP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
J301CP Injection Special Purpose GradeApplications: Cap of pressure bottleCharacteristics:High stiffnessSlip propertyInformation provided by Hyosung Corporation
Physical Properties Metric English Comments
Melt Flow 1.7 g/10 min
1.7 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 95
95
ASTM D785
Tensile Strength, Yield 40.2 MPa
5830 psi
ASTM D638
Elongation at Break 200 %
200 %
ASTM D638
Flexural Modulus 1.96 GPa
284 ksi
ASTM D790
Izod Impact, Unnotched 0.441 J/cm
0.827 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 125 °C
257 °F
ASTM D648
Vicat Softening Point 150 °C
302 °F
ASTM D1525