Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hyosung Topilene C600ME PP

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Hyosung Co.
Trade Name Topilene
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hyosung Topilene C600ME PP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
C600ME Butene Random CopolymerApplications: FilmCharacteristics:Excellent transparency & glossLow sealing temperatureHigh hot-tack strengthGood stiffnessInformation provided by Hyosung Corporation
Physical Properties Metric English Comments
Melt Flow 7.0 g/10 min
7.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.5 MPa
3840 psi
ASTM D638
Elongation at Break >= 500 %
>= 500 %
ASTM D638
Flexural Modulus 0.785 GPa
114 ksi
ASTM D790
Izod Impact, Unnotched 0.637 J/cm
1.19 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 133 °C
271 °F
Descriptive Properties Value Comments
Additives AB