Huntsman PE2067 Injection Molding Polyethylene  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman PE2067 Injection Molding Polyethylene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Homopolymer and FDA compliant.Features: High flow resin, provides excellent gloss and surface characteristics, and minimum cycle time.Applications: Injection molding: lids.FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (c)2.2 under condition of use B through H described in Table 2 of 21 CFR 176.170Information provided by Huntsman Corporation
Physical Properties Metric English Comments
Density 0.924 g/cc
0.0334 lb/in³
ASTM D1505
Melt Flow 35 g/10 min
35 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 55
55
ASTM D2240
Tensile Strength, Ultimate 10.0 MPa
1450 psi
ASTM D638
Tensile Strength, Yield 13.0 MPa
1890 psi
ASTM D638
Elongation at Break 200 %
200 %
ASTM D638
Modulus of Elasticity 0.345 GPa
50.0 ksi
Secant; ASTM D638
Thermal Properties Metric English Comments
Vicat Softening Point 98.0 °C
208 °F
ASTM D1525