Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hexcel® HexPly® 920 125°C Curing Epoxy Matrix

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Hexcel
Trade Name HexPly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® 920 125°C Curing Epoxy Matrix.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HexPly® 920 is a very tough advanced resin matrix, ideally suited to the single-shot production of honeycomb sandwich structures and the manufacture of solid laminates. It is highly tolerant of a variety of production techniques and equipments, making it easy to process. The high toughness of HexPly® 920 makes it ideal for industrial applications and performance cars. it is available preimpregnated into carbon, glass or aramid fibers.Information provided by HexCel
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
Cured
Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.9 MPa
5060 psi
ISO R527 type 1
Elongation at Yield 7.4 %
7.4 %
Compression Strain; ISO 604
8.41 %
8.41 %
ISO R527 type 1
Tensile Modulus 3.76 GPa
545 ksi
ISO R527 type 1
Flexural Modulus 3.51 GPa
509 ksi
ISO 178
Compressive Yield Strength 290 MPa
42100 psi
ISO 604
Poissons Ratio 0.39
0.39
ISO R527 type 1
Fracture Toughness 1.55 MPa-m½
1.41 ksi-in½
Shear Modulus 1.35 GPa
196 ksi
Calculated
Toughness 541 J
399 ft-lb
Per square meter
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 107 °C
225 °F
DMTA
Shrinkage 1.59 %
1.59 %
Processing Properties Metric English Comments
Shelf Life >= 12.0 Month

@Temperature -18.0 °C
>= 12.0 Month

@Temperature -0.400 °F
Descriptive Properties Value Comments
Tack Life (days) 30