Mechanical Properties Metric English Comments
Toughness 541 J
399 ft-lb
Per square meter
Hexcel® HexPly® 920 125°C Curing Epoxy Matrix
HexPly® 920 is a very tough advanced resin matrix, ideally suited to the single-shot production of honeycomb sandwich structures and the manufacture of solid laminates. It is highly tolerant of a v..