Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 107 °C | 225 °F | Average value: 107 °C Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m.. |
|||
Glass Transition Temp, Tg | 107 °C | 225 °F | 10°C/min test |
Polimeri Europa SINKRAL A22V ABS
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-25-09-25 Very high flow grade for fast cycle injection moulding. Particularly recommended for the domestic .. |
|||
Glass Transition Temp, Tg | 107 °C | 225 °F | 10°C/min test |
Polimeri Europa SINKRAL B813 ABS, Impact Grade
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-04-35-15 Injection moulding grade, providing very high impact resistance, even at low temperatures. Used as.. |
|||
Glass Transition Temp, Tg | 107 °C | 225 °F | |
Eastman Tenite 180A-28(HT) Cellulose Acetate
(discontinued **) 28% Plasticized.ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Glass Transition Temp, Tg | 107 °C | 225 °F | |
Eastman Tenite 264-10 CAB Cellulose Acetate Butyrate
(discontinued **) 10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Glass Transition Temp, Tg | 107 °C | 225 °F | ASTM D3418 |
Kolon DIAMAT® EG Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Glass Transition Temp, Tg | 107 °C | 225 °F | ASTM D3418 |
Styrolution Terlux® 2802 HD MABS Description: Terlux 2802 HD is a standard injection molding Methyl Methacrulate Acrylonitrile Butadiene Styrene grade for transparent parts.Information provided by STYROLUTION, which is a joint vent.. |
|||
Glass Transition Temp, Tg | 107 °C | 225 °F | 10 K/min; ISO 11357-1/-3 |
Styrolution Terlux® 2802 TR MABS Terlux 2802 TR is a standard injection molding MABS grade for tranparent parts.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Glass Transition Temp, Tg | 107 °C | 225 °F | 10 K/min; ISO 11357-1/-3 |
Styrolution Terlux® 2812 TR MABS Terlux 2812 TR is a transparent grade of MABS for injection molding with high flowability.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Glass Transition Temp, Tg | 107 °C | 225 °F | DMTA |
Hexcel® HexPly® 920 125°C Curing Epoxy Matrix HexPly® 920 is a very tough advanced resin matrix, ideally suited to the single-shot production of honeycomb sandwich structures and the manufacture of solid laminates. It is highly tolerant of a v.. |