Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Shear Modulus = 1.35 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 1.35 - 1.46 GPa
196 - 212 ksi
Calculated
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire PEEK is produced to the highest industry standards and is characterized by a dist..
Shear Modulus 1.35 GPa
196 ksi
ISO 6721-2
Styrolution Polystyrol 143 E GR 2 PS
Description: Polystyrol 143 E is a medium strength, easy flowing general purpose grade, suitable for blending with impact modified Polystyrol, Styrolux and coextruded gloss layers.Applications: In b..
Shear Modulus 1.35 GPa
196 ksi
ISO 6721-2
Styrolution Polystyrol 143 E GR 21 PS
Description: Polystyrol 143 E is a medium strength, easy flowing general purpose grade, suitable for blending with impact modified Polystyrol, Styrolux and coextruded gloss layers.Applications: In b..
Shear Modulus 1.35 GPa
196 ksi
ISO 6721-2
Styrolution Polystyrol 145 D PS
Description: Polystyrol 145 D is a medium strength, easy flowing general purpose grade, suitable for blending with impact modified Polystyrol.Applications: In blends with high impact polystyrene esp..
Shear Modulus 1.35 GPa
196 ksi
Calculated
Hexcel® HexPly® 920 125°C Curing Epoxy Matrix
HexPly® 920 is a very tough advanced resin matrix, ideally suited to the single-shot production of honeycomb sandwich structures and the manufacture of solid laminates. It is highly tolerant of a v..
Copyright © lookpolymers.com All Rights Reserved