A popular heat transfer salt for use in the higher temperature ranges. It is more inert to ferrous alloys than Partherm 290 or 350 and considerably lower in cost. Its heat capacity and thermal conductivity are at least as good. (430 Parkettes)Information provided by Heatbath Corporation - Park Metallurgical.
Thermal Properties Metric English Comments
Melting Point 221 °C
430 °F
Maximum Service Temperature, Air 593 °C
1100 °F
Upper limit of working range
Minimum Service Temperature, Air 121 °C
249 °F
Lower limit of working range