Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | 121 °C | 249 °F | Lower limit of working range |
Heatbath/Park Partherm 430 Heat Transfer Salt A popular heat transfer salt for use in the higher temperature ranges. It is more inert to ferrous alloys than Partherm 290 or 350 and considerably lower in cost. Its heat capacity and thermal cond.. |