Polymer Property : Tensile Strength, Ultimate = 45.1 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 45.1 MPa
6540 psi
ASTM D638
Hannam Chemical Hanalac 711 ABS, Plating Grade
Plating grade with excellent moldability and easy to surface treat. It also has a strong adhesive strength after plating and an excellent heat cycle. Applications: Appliances, TV frames, automoti..
Tensile Strength, Ultimate 45.1 MPa
6540 psi
ASTM D638
SK Chemicals SKYPEL M555CR Special Grade Copper Resistance
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
Tensile Strength, Ultimate 45.1 MPa
6540 psi
ASTM D638
SK Chemicals SKYPEL G168D General Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..