Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

HP Alloys Nitronic® 50 Austenitic Stainless, Level 4 Cold Worked

Category Metal , Ferrous Metal , Heat Resisting , Stainless Steel , T S20000 Series Stainless Steel
Manufacturer High Performance Alloys, Inc
Trade Name Nitronic®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF HP Alloys Nitronic® 50 Austenitic Stainless, Level 4 Cold Worked.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Cold Worked applies to tensile values and are for 1/4 to 2 in. diameter samples; other properties are typical of this alloy.Nitronic® 50 Stainless Steel provides a combination of corrosion resistance and strength not found in any other commercial material available in its price range. This austenitic stainless has corrosion resistance greater than that provided by Types 316 and 316L, plus approximately twice the yield strength at room temperature. In addition, Armco Nitronic 50 Stainless has very good mechanical properties at both elevated and sub-zero temperatures. And, unlike many austenitic stainless steels, Nitronic 50 does not become magnetic when cold worked.Data provided by High Performance Alloys, Inc.
Physical Properties Metric English Comments
Density 7.88 g/cc
0.285 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 1241 MPa
>= 180000 psi
Tensile Strength, Yield >= 1000 MPa

@Strain 0.200 %
>= 145000 psi

@Strain 0.200 %
Elongation at Break >= 12 %
>= 12 %
Reduction of Area >= 45 %
>= 45 %
Modulus of Elasticity 193 GPa
28000 ksi
In Tension
Charpy Impact 53.0 J

@Temperature -79.0 °C
39.1 ft-lb

@Temperature -110 °F
58.0 J

@Temperature -40.0 °C
42.8 ft-lb

@Temperature -40.0 °F
71.0 J

@Temperature 27.0 °C
52.4 ft-lb

@Temperature 80.6 °F
Thermal Properties Metric English Comments
CTE, linear 16.2 µm/m-°C

@Temperature 20.0 - 95.0 °C
9.00 µin/in-°F

@Temperature 68.0 - 203 °F
Component Elements Properties Metric English Comments
Chromium, Cr 22 %
22 %
Iron, Fe 58 %
58 %
as balance
Manganese, Mn 5.0 %
5.0 %
Molybdenum, Mo 2.25 %
2.25 %
Nickel, Ni 12.5 %
12.5 %
Nitrogen, N 0.30 %
0.30 %
Silicon, Si <= 1.0 %
<= 1.0 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.000110 ohm-cm
0.000110 ohm-cm