Polymer Property : Charpy Impact = 52.4 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact 71.0 J

@Temperature 25.0 °C
52.4 ft-lb

@Temperature 77.0 °F
Metal Sample from Plate Weld
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) All Weld Cruciform
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Charpy Impact 71.0 J

@Temperature 27.0 °C
52.4 ft-lb

@Temperature 80.6 °F
HP Alloys Nitronic® 50 Austenitic Stainless, Level 4 Cold Worked
Cold Worked applies to tensile values and are for 1/4 to 2 in. diameter samples; other properties are typical of this alloy.Nitronic® 50 Stainless Steel provides a combination of corrosion resist..