Gwent Electronic Materials R2040212D3 High Viscosity Acrylic Pressure Adhesive for Diagnostic Sensors

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Gwent Electronic Materials Ltd.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gwent Electronic Materials R2040212D3 High Viscosity Acrylic Pressure Adhesive for Diagnostic Sensors.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This material has a high viscosity, it is a water based acrylic pressure sensitive screen printable adhesive. It can be used in many different diagnostic applications such as test cards, assays and support systems for membrane-based immunodiagnostic tests. The adhesive is designed to be used in electrochemical sensors, electrochemical arrays and can be used for other adhesive purposes in building multilayer sensor systems.The paste is in a ready to use form at a viscosity suitable for automatic or semiautomatic screen printing.Information provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Solids Content 47 - 51 %
47 - 51 %
Viscosity 2100 - 2500 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
2100 - 2500 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Storage Temperature <= 25.0 °C
<= 77.0 °F
cool dry place
Processing Properties Metric English Comments
Processing Temperature 40.0 - 50.0 °C
104 - 122 °F
110 °C
230 °F
3-4 seconds to give a good heat seal
Shelf Life 3.00 Month
3.00 Month
Descriptive Properties Value Comments
Coverage m2/ltr 5