Polymer Property : Processing Temperature = 122 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 1632Z PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 1632Z is a general purpose, 15% fiberglass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability.15% glass-fiber, improved impactInformation p..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 1700FC PBT  (Unverified Data**)
Celanex 1700FC is a very high molecular weight extrusion grade of unreinforced polybutylene terephthalate for use in food contact applications.high molecular weight, unfilled PBT for use in food con..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 2000-3 PBT  (Unverified Data**)
Celanex 2000-3 is a general purpose, unreinforced PBT with a good balance of mechanical properties and processabillity.. Celanex 2000-3 is a high flow material. Celanex 2000-3 contains an internal..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 2001FC PBT  (Unverified Data**)
Celanex 2001FC is an unreinforced polybutylene terephthalate resin with improved hydrolysis resistance developed for use in fiber optic buffer tube applications for use in food contact applications...
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 2003HR PBT  (Unverified Data**)
Celanex 2003HR is an unfilled polybutylene terephthalate which has an excellent hydrolysis resistance, mechanical properties and processabilityHydrolytically stable / injectionInformation provided b..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 2300 GV3/20 PBT, 20% Glass Reinforced  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: PBT20% Glass bead reinforced gradeInformation provided by Celanese
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 2300 GV3/30 PBT, 30% Glass Reinforced  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: PBT30% Glass bead reinforced gradeInformation provided by Celanese
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 2401 MT PBT, Medical Technology  (Unverified Data**)
Celanex 2401 MT Natural is an unreinforced, high molecular weight PBT that complies with the requirements of CFR 21 177.1660 of the Food and Drug Administration (FDA) and is listed in the Drug Maste..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 3309HRLM PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3309HRLM is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and processability.30% glass filled PBT, h..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 3400-2 PBT, 40% Glass Reinforced  (Unverified Data**)
Celanex 3400-2 is a general purpose, 40% glass reinforced polybutylene terephthalate that offers a good combination of mechanical, electrical, and thermal properties. This grade provides outstanding..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 4022 PBT, Specialty  (Unverified Data**)
A white PBT resin typically used for applications requiring very opaque parts.PBT, opaque whiteInformation provided by Celanese
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 4300FC PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 4300FC is a toughened, 30% glass reinforced PBT for use in food contact applications.30% glass reinforced PBT for use in food contact applicationsInformation provided by Celanese
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 4302LM PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 4302 is a 30% glass reinforced PBT designed for improved mold flow, warp resistance and surface appearance, that is also enhanced for improved laser marking graphics.30% glass fiber, impact ..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 4306 PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 4306 is a 30% glass reinforced, toughened, low warpage thermoplastic polyester.30% glass-fiber, impact modified, low warpInformation provided by Celanese
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 5202 PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 5202 is a 15% glass filled polyester that features improved surface gloss and has an excellent balance of mechanical properties, processability, and color stability under heat and UV exposur..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 531HS PBT, Glass Reinforced  (Unverified Data**)
Celanex 531HS is a 30% fiberglass reinforced PBT which has an excellent balance of mechanical properties and processability. Celanex 531HS is specifically designed to exhibit excellent thermal shoc..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 6500 PBT, 30% Mineral / Glass Reinforced  (Unverified Data**)
Celanex 6500 is a 30% glass/mineral polyester with improved surface finish and a good balance of mechanical properties and processability.30% glass/mineral, low warpInformation provided by Celanese
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Vandar® 4602Z PBT  (Unverified Data**)
4602Z is an unfilled thermoplastic alloy with good weatherability and chemical resistance.Unreinforced, good chemical resistanceInformation provided by Celanese
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Vandar® 4632Z PBT, 15% Glass Reinforced  (Unverified Data**)
Vandar 4632Z is a high impact, 15% glass reinforced polyester alloy. It combines high strength and toughness with a moderate degree of rigidity. It is characterized by excellent solvent resistance, ..
Processing Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Both A and B components
Taiwan PU Corporation CPU-69-A/B Polyurethane Casting Elastomer
CPU-69-A consists of polyether polyols and other additives. CPU-69-b is an isocyanate prepolymer. Together they create compounds that cure under room temperature and have short working times, shor..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
hopper
Celanese Celanex® 1662Z PBT, 30% Glass Reinforced
Celanex 1662Z is a 30% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processabilityTo avoid hydrolytic degradation during processing, CELANEX resins ha..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
hopper
Celanese Celanex® 3200 PBT, 15% Glass Reinforced
Celanex 3200 is a general purpose, 15% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability.To avoid hydrolytic degradation during processing, ..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
hopper
Celanese Celanex® 3201 PBT, 15% Glass Reinforced
Celanex 3201 is a 15% glass reinforced general purpose thermoplastic polyester resin that offers a superior combination of mechanical, electrical, and thermal properties, together with outstanding p..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
hopper
Celanese Celanex® 3314 PBT, 30% Glass Reinforced
Celanex 3314 is a non-exuding (UL approved V-0 at 1/64 inch), 30% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechanical properties and processability. It is w..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
hopper
Celanese Celanex® 2002UV PBT, Unfilled
Celanex 2002UV is a general purpose,unreinforced polybutylene terephthalate with a good balance of mechanical properties, processability and UV resistance. Celanex 2002UV is a medium flow materialTo..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 2002-2 PBT  (Unverified Data**)
Celanex 2002-2 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 2002-2 ia a medium flow material that contains a..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 3300D PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3300D is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outsta..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 6407 PBT, 30% Mineral / Glass Reinforced  (Unverified Data**)
Celanex 6407 is a 30% glass/mineral reinforced resin perticularly suited for large exterior automotive components, where extended flow, flatness and good surface appearance is essential.30% glass/mi..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Impet® 830R PET, 35% Mineral / Glass Reinforced  (Unverified Data**)
Impet 830R is a 35% glass/mineral reinforced injection moldable polyester made with recycled PET. It provides an excellent combination of strength, stiffness, warp resistance, and high temperature c..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
hopper
Celanese Celanex® 3116 PBT, 7.5% Glass Reinforced
Celanex 3116 is a non-exuding flame retarded (UL and CSA approved V-0 at 1/32 inch and 5V at 1/8 inch), 7.5% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechan..