Polymer Property : Processing Temperature = 50.0 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 1462Z PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 1462Z is a general purpose, 30% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability.30% glass-fiber, general purposeInformation provid..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 1602Z PBT  (Unverified Data**)
Celanex 1602Z is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 1602Z has an internal lubricant.Lubricated extrus..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 1632Z PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 1632Z is a general purpose, 15% fiberglass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability.15% glass-fiber, improved impactInformation p..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 1700FC PBT  (Unverified Data**)
Celanex 1700FC is a very high molecular weight extrusion grade of unreinforced polybutylene terephthalate for use in food contact applications.high molecular weight, unfilled PBT for use in food con..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 2008 PBT  (Unverified Data**)
Celanex 2008 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in melt blown applications.Ultrahigh melt flowInfor..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 2300 GV3/20 PBT, 20% Glass Reinforced  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: PBT20% Glass bead reinforced gradeInformation provided by Celanese
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 3216 PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 3216 is a non-exuding (UL and CSA approved V-0 at 1/32 inch and 5V at 1/8 inch ),15% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechanical properties ..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 3300 PBT, 30% Glass Reinforced  (Unverified Data**)
Ceanex 3300 is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outstandi..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 3425HRT PBT, Glass Reinforced  (Unverified Data**)
Celanex 3425HRT is a non-lubricated, 40% fiberglass reinforced PBT copolymer that has excellent hydrolysis resistance, toughness, improved flow, and improved elongation at break.40% fiberglass reinf..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 4202 PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 4202 is a 15% glass reinforced, impact modified polybutylene terephthalate with excellent surface appearance.15% glass-fiber, improved impactInformation provided by Celanese
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 4300 PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 4300 is a toughened, 30% glass reinforced PBT.30% glass-fiber, good impact strengthInformation provided by Celanese
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 4300LM PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 4300LM is a toughened 30% glass reinforced PBT that is enhanced for improved laser marking graphics.30% glass fiber, good impact strength, laser markableInformation provided by Celanese
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 4302 PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 4302 is a 30% glass reinforced PBT designed for improved mold flow, warp resistance and surface appearance.30% glass-fiber, impact modifiedInformation provided by Celanese
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 4306 PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 4306 is a 30% glass reinforced, toughened, low warpage thermoplastic polyester.30% glass-fiber, impact modified, low warpInformation provided by Celanese
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 5200-2 PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 5200-2 is a 15% fiberglass reinforced polyester with improved surface finish. Celanex 5200-2 contains an internal lubricant.15% glass reinforced, high gloss, general purpose, lubricatedInfor..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Vandar® 2500 PBT  (Unverified Data**)
Vandar 2500 is an unfilled polyester alloy which exhibits excellent toughness and impact strength. It is specially designed to offer excellent chemical resistance, good colorability and dimensional ..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Vandar® 4612R PBT, 7% Glass Reinforced  (Unverified Data**)
Vandar 4612R is a high impact polyester alloy containing 7% glass. It possesses excellent impact properties as well as toughness and moldability. Dimensional stability, chemical resistance, and low ..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Vandar® 4662Z PBT, 30% Glass Reinforced  (Unverified Data**)
Vandar 4662Zis a high impact polyester alloy which contains 30% glass fiber loading. It is characterized by toughness, dimensional stability, and high modulus. Good weatherability and moldability ar..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Vandar® 8000 PBT  (Unverified Data**)
Vandar 8000 polyester alloy is designed to meet UL94 V-0 requirements at 1/32 inch thickness while retaining excellent impact resistance. The product is characterized by excellent moldability and su..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Impet® 2700 GV1/45 (Europe) PET, 45% Glass Reinforced  (Unverified Data**)
Polyethylene terephthalate, 45 % glass filled, high flowability, excellent gloss, high modulus, very high heat deflection temperature.45% glass fiber reinforcedInformation provided by Celanese
Processing Temperature 40.0 - 50.0 °C
104 - 122 °F
Gwent Electronic Materials R2040212D3 High Viscosity Acrylic Pressure Adhesive for Diagnostic Sensors
This material has a high viscosity, it is a water based acrylic pressure sensitive screen printable adhesive. It can be used in many different diagnostic applications such as test cards, assays and..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 3109HR PBT, 7.5% Glass Reinforced
Celanex 3109HR is a non-lubricated, 7.5% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties, and processability.7.5% glass filledInform..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
hopper
Celanese Celanex® 3209HR PBT, Glass Reinforced
Celanex 3209HR is a 15% glass filled PBT that has an excellent hydrolysis resistance, mechanical properties and processability. Celanex 3209HR is non-lubricated.Information provided by Celanese Cor..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
hopper
Celanese Celanex® 4305 PBT, 33% Glass Reinforced
Celanex 4305 is a 33% glass reinforced, toughened, thermoplastic polyester.To avoid hydrolytic degradation during processing, CELANEX resins have to be dried to a moisture level equal to or less tha..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
hopper
Celanese Celanex® 5214HF PBT, 15% Glass Reinforced
Celanex 5214HF is a high flow, 15% glass reinforced, high gloss, flame retardant polyester.Pre-drying: 250F (120C) for 4 HoursInformation provided by Celanese Corporation.
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
hopper
Celanese Celanex® 3200HR PBT, 15% Glass Reinforced
Celanex 3200HR is a 15% glass filled polybutylene terephthalate which has an excellent hydrolysis resistance, mechanical properties and processability.To avoid hydrolytic degradation during processi..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
hopper
Celanese Celanex® 6406 PBT, 40% Mineral / Glass Reinforced
Celanex 6406 is a 40% mineral/glass reinforced resin providing excellent toughness combined with warpage resistance, surface gloss and good mechanical properties. Celanex 6406 is particularly suited..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celanex® 6407 PBT, 30% Mineral / Glass Reinforced  (Unverified Data**)
Celanex 6407 is a 30% glass/mineral reinforced resin perticularly suited for large exterior automotive components, where extended flow, flatness and good surface appearance is essential.30% glass/mi..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Impet® 340R PET, 45% Glass Reinforced  (Unverified Data**)
Impet 340R is a 45% glass-reinforced injection moldable polyester made with post consumer recycled PET. It provides an excellent combination of strength, stiffness, and high temperature resistance.4..
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
hopper
Celanese Celanex® 3116 PBT, 7.5% Glass Reinforced
Celanex 3116 is a non-exuding flame retarded (UL and CSA approved V-0 at 1/32 inch and 5V at 1/8 inch), 7.5% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechan..