Gwent Electronic Materials C2030812D3 Silver/Silver Chloride Paste

Category Fluid , Metal , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Gwent Electronic Materials Ltd.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gwent Electronic Materials C2030812D3 Silver/Silver Chloride Paste.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Silver/Silver Chloride Paste has a ratio of Silver to Silver Chloride of 60/40. Applications in medical diagnostics, environmentalScreen Printing Equipment: semi-automatic, manualScreen Types: polyester, mesh 156-230tpiSubstrate: Polyester, PVC, Polycarbonate or ceramic Note: Stainless steel mesh is not recommended, since a paste component can become corrosive in the presence of moisture. Also, plastic palette knives should be used instead of metal knives.Information provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Solids Content 81.14 - 83.14 %

@Temperature 130 °C
81.14 - 83.14 %

@Temperature 266 °F
Viscosity 3500 - 7000 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
3500 - 7000 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Thickness 16.0 microns
0.630 mil
Cured, Typical, Using a 156 mesh stainless steel screen, 13 micron emulsion
Storage Temperature 20.0 °C
68.0 °F
sealed container
Electrical Properties Metric English Comments
Surface Resistivity per Square 0.50 ohm
0.50 ohm
Using a 156 mesh stainless steel screen, 13 micron emulsion
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 80.0 °C
0.167 hour

@Temperature 176 °F
30.0 min

@Temperature 60.0 °C
0.500 hour

@Temperature 140 °F
Shelf Life 3.00 Month
3.00 Month
Descriptive Properties Value Comments
Coverage cm2/g 130
Using a 230 mesh stainless steel screen