Material Notes:
Greene Tweed’s WR® FP100, a reinforced compression-molded polyketone, offers excellent wear resistance with FDA compliance. The typical properties and physical characteristics of WR FP100 make it well suited for use as bushings and wear rings in rotating equipment.WR FP100’s FDA compliance allows it to be used in pump applications for drinking water, food processing and pharmaceutical manufacturing.Information provided by Greene Tweed.
Physical Properties Metric English Comments
Specific Gravity 1.52 g/cc
1.52 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell M 97
97
ASTM D785
Hardness, Shore D 89
89
ASTM D2240
Tensile Strength at Break 68.27 MPa
9902 psi
ASTM D638
Elongation at Break 3.5 %
3.5 %
ASTM D1457
Flexural Strength 148.16 MPa
21489 psi
ASTM D790
Flexural Modulus 6.446 GPa
934.8 ksi
Flexural 0.5% Secant Modulus; ASTM D790
Compressive Strength 222.51 MPa
32272 psi
ASTM D695
Secant Modulus 6.15 GPa
892 ksi
Tensile 0.5% Secant Modulus; ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 135 °C
275 °F
Minimum Service Temperature, Air -73.3 °C
-100 °F
Descriptive Properties Value Comments
Color Tan