Tensile Strength at Break 68.27 MPa
9902 psi
ASTM D638
Greene Tweed WRâ„¢ FP100 Polyketone, Reinforced
Greene Tweed’s WR® FP100, a reinforced compression-molded polyketone, offers excellent wear resistance with FDA compliance. The typical properties and physical characteristics of WR FP100 m..