Mechanical Properties Metric English Comments
Compressive Strength 222.51 MPa
32272 psi
ASTM D695
Greene Tweed WRâ„¢ FP100 Polyketone, Reinforced
Greene Tweed’s WR® FP100, a reinforced compression-molded polyketone, offers excellent wear resistance with FDA compliance. The typical properties and physical characteristics of WR FP100 m..