Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 11.20 MPa | 1625 psi | @100% Elongation; ASTM D1414 |
Greene Tweed Fluoroelastomer 931 FKM Fluoroelastomer 931 performs well in aggressive chemical where ultrapure materials are not required. Recommended for conventional wet and dry system applications, Fluoroelastomer 931 has a good fie.. |