Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 95.98 MPa | 13920 psi | Transverse; ASTM D732 |
Greene Tweed Arlon® 1286 Polyketone, Carbon Filled Greene Tweed offers precision plastic components for a variety of demanding semiconductor applications. These components are made from a full range of high-performance plastic materials including A.. |