Gouda Vuurvast CURON 160 H SIC GM Dense Refractory Castable

Category Ceramic , Carbide , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Gouda Vuurvast
Trade Name CURON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast CURON 160 H SIC GM Dense Refractory Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: This gunning castable has an extremely good thermal shock resistance and very good resistance against aggressive slags. Application among others in the copper industry.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.15 - 2.25 g/cc
0.0777 - 0.0813 lb/in³
After drying at 110°C
Particle Size <= 6000 µm
<= 6000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 25.0 - 35.0 MPa

@Temperature 1300 °C
3630 - 5080 psi

@Temperature 2370 °F
Cold Crushing Strength
35.0 - 45.0 MPa

@Temperature 100 °C
5080 - 6530 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.810 - 0.910 W/m-K

@Temperature 100 °C
5.62 - 6.32 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.810 - 0.910 W/m-K

@Temperature 600 °C
5.62 - 6.32 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.890 - 1.09 W/m-K

@Temperature 1300 °C
6.18 - 7.56 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Maximum Service Temperature, Air 1600 °C
2910 °F
Shrinkage -0.250 - 0.250 %

@Temperature 1300 °C
-0.250 - 0.250 %

@Temperature 2370 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 58 %
58 %
Fe2O3 <= 1.5 %
<= 1.5 %
SiC 10 %
10 %
SiO2 26 %
26 %
Descriptive Properties Value Comments
ASTM Classification E
Material Consumption per 1 m3 2150 kg