Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.810 - 0.910 W/m-K @Temperature 100 °C |
5.62 - 6.32 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 160 H SIC GM Dense Refractory Castable Description: This gunning castable has an extremely good thermal shock resistance and very good resistance against aggressive slags. Application among others in the copper industry.Remarks: These va.. |
|||
Thermal Conductivity | 0.810 - 0.910 W/m-K @Temperature 600 °C |
5.62 - 6.32 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 160 H SIC GM Dense Refractory Castable Description: This gunning castable has an extremely good thermal shock resistance and very good resistance against aggressive slags. Application among others in the copper industry.Remarks: These va.. |
|||
Thermal Conductivity | 0.810 - 0.910 W/m-K @Temperature 1300 °C |
5.62 - 6.32 BTU-in/hr-ft²-°F @Temperature 2370 °F |
|
Gouda Vuurvast CURON 165 GM Dense Refractory Castable Description: Curon 165 GM is based on bauxite and very pure chamotte grog. In has very good thermal shock resistance and a low firing shrinkage.Remarks: These values apply to cast products. Other mo.. |