Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 2.15 - 2.25 g/cc | 0.0777 - 0.0813 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 127 S Dense Refractory Castable Description: Curon 127 S castable is characterized by a very high strength and a good resistance against slag attack. This castable is applied mainly in boilers and incinerators.Remarks: These value.. |
|||
Bulk Density | 2.15 - 2.25 g/cc | 0.0777 - 0.0813 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 150 HS Dense Refractory Castable Description: Dense refractory castableRemarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information provided by Gouda Vuurvast. |
|||
Bulk Density | 2.15 - 2.25 g/cc | 0.0777 - 0.0813 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 150 HS GM Dense Refractory Castable Description: Curon 150 HS GM is an abrasion resistant gunning castable for use up to 1500°C.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast. |
|||
Bulk Density | 2.15 - 2.25 g/cc | 0.0777 - 0.0813 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 160 H SIC GM Dense Refractory Castable Description: This gunning castable has an extremely good thermal shock resistance and very good resistance against aggressive slags. Application among others in the copper industry.Remarks: These va.. |
|||
Bulk Density | 2.15 - 2.25 g/cc | 0.0777 - 0.0813 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURAS 40 D Moldable Refractory Material Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. Because of special additions this type of moldable has already a reasonabl.. |
|||
Bulk Density | 2.15 - 2.25 g/cc | 0.0777 - 0.0813 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURAS 40 PD Moldable Refractory Material Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. Because of the addition of phosphate this type of moldable has a high stre.. |
|||
Bulk Density | 2.15 - 2.25 g/cc | 0.0777 - 0.0813 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURAS 60 SD Moldable Refractory Material Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. Because this material contains a high percentage of sillimanite, it has a .. |
|||
Bulk Density | 2.15 - 2.25 g/cc | 0.0777 - 0.0813 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 145 C Dense Refractory Castable Description: A low carbon castable for use in reducing atmospheres. Curon 145 C has a coarse structure for improved thermal shock resistance.Remarks: These values apply to cast products.Information .. |
|||
Bulk Density | 2.15 - 2.25 g/cc | 0.0777 - 0.0813 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 145 Dense Refractory Castable Description: Because of the use of pure raw materials, Curon 145 has a low Fe2O3 content. Therefore this castable is widely used in reducing atmospheres.Remarks: These values apply to cast products... |
|||
Bulk Density | 2.15 g/cc | 0.0777 lb/in³ | |
Chosun Refractories AC-2 Acid-Proof and Heat-Resistant Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.15 g/cc | 0.0777 lb/in³ | |
Chosun Refractories AH-4 Acid-Proof and Heat-Resistant Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.15 g/cc | 0.0777 lb/in³ | |
Chosun Refractories N2-2 Fireclay brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.15 g/cc | 0.0777 lb/in³ | |
Chosun Refractories N3-1 Fireclay brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.15 g/cc | 0.0777 lb/in³ | |
Chosun Refractories SF31 Hard Fireclay brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.15 g/cc | 0.0777 lb/in³ | |
Chosun Refractories AH-1 Acid-Proof and Heat-Resistant Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.15 g/cc | 0.0777 lb/in³ | |
Chosun Refractories N4-1 Fireclay brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |