Material Notes:
Description: This brick has a low porosity and a high strength and therefore a very good slag resistance. Applications: rotary cement kilns.Remarks: This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Density 2.35 g/cc
0.0849 lb/in³
Apparent
Porosity 15 %
15 %
Apparent
Mechanical Properties Metric English Comments
Compressive Strength 50.0 MPa
7250 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 1.51 W/m-K

@Temperature 100 °C
10.5 BTU-in/hr-ft²-°F

@Temperature 212 °F
1.59 W/m-K

@Temperature 650 °C
11.0 BTU-in/hr-ft²-°F

@Temperature 1200 °F
1.67 W/m-K

@Temperature 1100 °C
11.6 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Maximum Service Temperature, Air 1500 °C
2730 °F
1520 °C
2770 °F
Deformation under load - t<sub>a</sub>
Component Elements Properties Metric English Comments
Al2O3 50 %
50 %
Fe2O3 1.5 %
1.5 %
SiO2 43 %
43 %
Descriptive Properties Value Comments
Segercone 35
Thermal Shock Resistance 20 cycles
DIN 51068