Material Notes:
Features: Excellent processability, nucleated and antistat. Product does not contain animal derived components. Phthalate-free.Applications: Injection Molding: Cutlery, Consumer Products, Cosmetic Packaging, Caps and ClosuresInformation Provided by Flint Hills Resources
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 35 g/10 min
35 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D785
Tensile Strength, Yield 39.0 MPa
5660 psi
ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
Flexural Modulus, 1% Secant 1590 MPa
231000 psi
ASTM D790
Izod Impact, Notched 0.200 J/cm

@Temperature 23.0 °C
0.375 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Gardner Impact 6.00 J

@Temperature 23.0 °C
4.43 ft-lb

@Temperature 73.4 °F
ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 111 °C
232 °F
ASTM D648