Fainplast Compounds HAX HF 087/2 Halogen Free PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Fainplast Compounds
Trade Name HAX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds HAX HF 087/2 Halogen Free PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Filling and bedding
Physical Properties Metric English Comments
Density 1.88 - 1.92 g/cc
0.0679 - 0.0694 lb/in³
IEC 60811
Mechanical Properties Metric English Comments
Hardness, Shore D 34 - 40
34 - 40
IEC 60811
Thermal Properties Metric English Comments
Oxygen Index 35 - 45 %
35 - 45 %
ISO 4589
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+13 ohm-cm

@Temperature 20.0 °C
>= 1.00e+13 ohm-cm

@Temperature 68.0 °F
ASTM D257