Material Notes:
High fire performances, good flexibility
Physical Properties Metric English Comments
Density 1.58 - 1.62 g/cc
0.0571 - 0.0585 lb/in³
IEC 60811
Melt Index of Compound 2.0 g/10 min

@Load 21.6 kg,
Temperature 150 °C
2.0 g/10 min

@Load 47.6 lb,
Temperature 302 °F
Fainplast
Mechanical Properties Metric English Comments
Hardness, Shore D 42 - 48
42 - 48
IEC 60811
Tensile Strength at Break 10.0 MPa
1450 psi
IEC 60811
Elongation at Break 170 %
170 %
IEC 60811
Thermal Properties Metric English Comments
Oxygen Index 45 %
45 %
ISO 4589
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm

@Temperature 20.0 °C
1.00e+14 ohm-cm

@Temperature 68.0 °F
ASTM D257