ExxonMobil Santoprene® 221-87W211 Thermoplastic Elastomer  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Santoprene® 221-87W211 Thermoplastic Elastomer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A hard, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range of applications. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding, extrusion or blow molding. It is polyolefin based and completely recyclable.Formulated for good UV resistance and colorfastness. Information provided by Advanced Elastomer Systems
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 87
87
.12 in; ASTM D2240
Tensile Strength at Break 8.874 MPa
1287 psi
Air at 275°F, 1008 hr; ASTM D573
8.96 MPa
1300 psi
Across Flow; ASTM D412
Tensile Strength, Ultimate 6.07 MPa
880 psi
Across Flow; ASTM D412
Elongation at Break 328.5 %
328.5 %
Air at 275°F, 1008 hr; ASTM D573
450 %
450 %
Across Flow; ASTM D412
Processing Properties Metric English Comments
Processing Temperature 175 - 230 °C
347 - 446 °F
Descriptive Properties Value Comments
Color Natural Color
Form Pellets