Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 8.96 MPa | 1300 psi | TM R050-36 |
Resinlab® EP1225 Black Unfilled Epoxy Adhesive Resinlab™ EP1225 Black is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. It has slightly thixotropic viscosity to give gap filling ability bust stil.. |
|||
Tensile Strength at Break | 8.96 MPa @Temperature 23.0 °C |
1300 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7430-9001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7430-9001-00 is an easy processing, high performance compound designed for use in applications requiring tough, durable material. - Excellent Heat Stability - Good Ozone and UV Stability.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R1765K Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R5155A White 759 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | 20 in/min; ASTM D638 |
LyondellBasell Microthene® MP574189 Linear Low Density Polyethylene, Injection Molding Grade ApplicationsMicrothene MP574189 exhibits excellent flow and impact with good stiffness. Typical applications include lids, closures, containers, housewares and medical items. MP574189 is 16 mesh pow.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D1414 |
Greene Tweed CHEMRAZ® 584 Perfluoroelastomer Greene Tweed’s Chemraz® 584, a cream-colored perfluoroelastomer, is a specialty compound formulated to outlast the most demanding chemical process applications. Because of its outstanding o.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | Crosshead Speed - 20 in/min; ASTM D638 |
LyondellBasell Petrothene® NA870252 Low Density Polyethylene ApplicationsPETROTHENE NA 870-252 exhibits an excellent balance of toughness and softness, with excellent dimensional stability. Typical applications include caps and closures, housewares, toys, co.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D412 |
Teknor Apex Monprene® MP 1023 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D412 |
Teknor Apex Monprene® MP 1037FL Thermoplastic Elastomer Notes: Transparent Features: High FlowInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D412 |
Teknor Apex Monprene® MP 1851 Thermoplastic Elastomer Notes: Translucent Features: High FlowInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D412 |
Teknor Apex Monprene® MP-1564-L1 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D412 |
Teknor Apex Monprene® MP-1564L3 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D412 |
Teknor Apex Monprene® MP-2120 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D412 |
Teknor Apex Monprene® MP-2322UV Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D412 |
Teknor Apex Monprene® MP-2579A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D412 |
Teknor Apex Monprene® MP-2581A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D412 |
Teknor Apex Monprene® MP-3017 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D412 |
Teknor Apex Telcar® TL-1137 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D412 |
Teknor Apex Telcar® TL-1642E Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D638 |
ExxonMobil HDPE HD 6706.17 High Density Polyethylene Copolymer Resin Product Description: HD 6706 is a narrow molecular weight hexane copolymer designed for good processability and excellent balance of ESR, Toughness and Stiffness properties. This resin is ideally su.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D638 |
ExxonMobil HDPE HD 6706.62 High Density Polyethylene Copolymer Resin Product Description: HD 6706 is a narrow molecular weight hexane copolymer designed for good processability and excellent balance of ESR, Toughness and Stiffness properties. This resin is ideally su.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D638 |
Entec Hypel® PELD50/.924 LDPE Available in North America Features: Food Contact Acceptable and Low DensityAgency Ratings: FDA 21 CFR 176.170, Table 2, Cond. B; Cond. C; Cond. D; Cond. E; Cond. F; Cond. G; Cond. H; and FDA 21 CF.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D412 |
DuPont Performance Polymers Kalrez® Spectrum™ 0040 Fluoroelastomer Kalrez® Spectrum™ 0040 perfluoroelastomer parts are specifically designed for low-temperature environments where significant chemical resistance is required. Proprietary polymer and cure technolog.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D412 |
Teknor Apex Monprene® MP-2850M L2 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D412 |
Teknor Apex Monprene® MP 1037 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D412 |
Teknor Apex Monprene® MP-2875M Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |