Polymer Property : Tensile Strength at Break = 8.96 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 8.96 MPa
1300 psi
TM R050-36
Resinlab® EP1225 Black Unfilled Epoxy Adhesive
Resinlab™ EP1225 Black is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. It has slightly thixotropic viscosity to give gap filling ability bust stil..
Tensile Strength at Break 8.96 MPa
1300 psi
51 mm/min; ASTM D638
PolyOne Maxxam™ FR WC-P85 NHFR RoHS Natural Polyolefin, Unspecified
Maxxam™ HFFR WC-P85 RoHS Natural is a halogen-free flame retardant polyolefin compound characterized by low smoke, low flame spread, excellent spring-back, no plate-out and high extrusion line spee..
Tensile Strength at Break 8.96 MPa
1300 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible R5155A White 759 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength at Break 8.96 MPa
1300 psi
20 in/min; ASTM D638
LyondellBasell Microthene® MP574189 Linear Low Density Polyethylene, Injection Molding Grade
ApplicationsMicrothene MP574189 exhibits excellent flow and impact with good stiffness. Typical applications include lids, closures, containers, housewares and medical items. MP574189 is 16 mesh pow..
Tensile Strength at Break 8.96 MPa
1300 psi
ASTM D1414
Greene Tweed CHEMRAZ® 584 Perfluoroelastomer
Greene Tweed’s Chemraz® 584, a cream-colored perfluoroelastomer, is a specialty compound formulated to outlast the most demanding chemical process applications. Because of its outstanding o..
Tensile Strength at Break 8.96 MPa
1300 psi
Crosshead Speed - 20 in/min; ASTM D638
LyondellBasell Petrothene® NA870252 Low Density Polyethylene
ApplicationsPETROTHENE NA 870-252 exhibits an excellent balance of toughness and softness, with excellent dimensional stability. Typical applications include caps and closures, housewares, toys, co..
Tensile Strength at Break >= 8.96 MPa
>= 1300 psi
ASTM D412 Method A
Seals Eastern 5722 Fluorocarbon-Elastomer
Formulated Viton®. General service.Information provided by Seals Eastern, Inc.
Tensile Strength at Break 8.96 MPa
1300 psi
ASTM D412
Teknor Apex Monprene® MP 1023 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 8.96 MPa
1300 psi
ASTM D412
Teknor Apex Monprene® MP 1851 Thermoplastic Elastomer
Notes: Translucent Features: High FlowInformation Provided by Teknor Apex
Tensile Strength at Break 8.96 MPa
1300 psi
ASTM D412
Teknor Apex Monprene® MP-1564L2 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 8.96 MPa
1300 psi
ASTM D412
Teknor Apex Monprene® MP-1695L1 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 8.96 MPa
1300 psi
ASTM D412
Teknor Apex Monprene® MP-1848 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 8.96 MPa
1300 psi
ASTM D412
Teknor Apex Monprene® MP-2357-A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 8.96 MPa
1300 psi
ASTM D412
Teknor Apex Monprene® MP 1304S Thermoplastic Elastomer
Uses: Grips Features: Good Resistance to Skin OilsInformation Provided by Teknor Apex
Tensile Strength at Break 8.96 MPa
1300 psi
ASTM D412
Teknor Apex Monprene® MP-2579A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 8.96 MPa
1300 psi
ASTM D412
Teknor Apex Monprene® MP-2850M Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 8.96 MPa
1300 psi
ASTM D412
Teknor Apex Monprene® MP-3017 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 8.96 MPa
1300 psi
ASTM D412
Teknor Apex Telcar® TL-1137 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Tensile Strength at Break 8.96 MPa
1300 psi
ASTM D638
ExxonMobil HDPE HD 6706.17 High Density Polyethylene Copolymer Resin
Product Description: HD 6706 is a narrow molecular weight hexane copolymer designed for good processability and excellent balance of ESR, Toughness and Stiffness properties. This resin is ideally su..
Tensile Strength at Break 8.96 MPa
1300 psi
ISO 527-2/1A/50
ExxonMobil LDPE LD 600BA Low Density Polyethylene Resin (European Grade)
Product Description: LD 600BA is a high flow LDPE grade, characterized by high stiffness and good toughness. It’s easy processable.Availability: Africa & Middle East and Europe Additive: Antiblock..
Tensile Strength at Break 8.96 MPa
1300 psi
Molded and tested in accordance with ASTM D4976; ASTM D638
Dow DNDA-1081 NT 7 Linear Low Density Polyethylene Resin
DOW DNDA-1081 NT 7 is produced using UNIPOL™ PE process technology. It is intended for high-speed injection molding of thin walled parts such as downguaged lids. Information provided by Dow
Tensile Strength at Break 8.96 MPa
1300 psi
Molded and tested in accordance with ASTM D4976; ASTM D638
Dow DNDA-1082 NT 7 Linear Low Density Polyethylene Resin
DOW DNDA-1082 NT 7 is produced using UNIPOL™ PE process technology. It is intended for high-speed injection molding of thin walled parts such as downguaged lids. Information provided by Dow
Tensile Strength at Break 8.96 MPa
1300 psi
ASTM D412
DuPont Performance Polymers Kalrez® Spectrum™ 0040 Fluoroelastomer
Kalrez® Spectrum™ 0040 perfluoroelastomer parts are specifically designed for low-temperature environments where significant chemical resistance is required. Proprietary polymer and cure technolog..
Tensile Strength at Break 8.96 MPa
1300 psi
ASTM D638
ExxonMobil Escorene™ LD 706.15 Molding Ethylene Vinyl Acetate Copolymer
Product Description: Escorene Ultra LD 706.15 is a 14.9 wt% vinyl acetate copolymer film resin designed for specialty molding, extrusion and compounding applications.Availability: Latin America, Nor..
Tensile Strength at Break 8.96 MPa
1300 psi
ASTM D412
Teknor Apex Monprene® MP 1579 Thermoplastic Elastomer
Notes: Translucent Features: Good Chemical and Oil Resistance; Tough; Good Melt StrengthInformation Provided by Teknor Apex
Tensile Strength at Break 8.96 MPa
1300 psi
TM R050-36
Resinlab® EP1026R Rubber Modified Epoxy Adhesive
Resinlab™ EP1026R is a two part unfilled rubber modified epoxy adhesive designed for high speed bonding of metals, ceramics, and most plastics. It cures to a tough semi-rigid material, and is free ..
Tensile Strength at Break 8.96 MPa
1300 psi
ASTM D412
Teknor Apex Monprene® MP 1037 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 8.96 MPa
1300 psi
ASTM D412
Compuestos Dominicanos Polycom CE-103165 PVC
Description: Compuestos Dominicanos, S.A. produces a wide variety of PVC compounds for the injection molding of foot wear products, everything from full injection, shoe soles, boots, and PVC compoun..
Tensile Strength at Break 8.96 MPa
1300 psi
ASTM D412
Teknor Apex Monprene® MP-2850M-UV Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..