Material Notes:
Product Description: A medium impact strength copolymer resin designed for injection-molded automotive applications requiring medium melt flow rate.Availability: North America Features:Impact ModifiedMedium FlowMedium Impact ResistanceUses: Automotive ApplicationsCompoundingConsumer ApplicationsToysProcessing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ExxonMobil Method
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.2 MPa
3220 psi
2.0 in/min; ASTM D638
Elongation at Yield 6.2 %
6.2 %
2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 1030 MPa
150000 psi
0.05 in/min; ASTM D790A
1180 MPa
171000 psi
0.5 in/min; ASTM D790B
Izod Impact, Notched 1.76 J/cm
3.30 ft-lb/in
ASTM D256A
Gardner Impact 24.0 J

@Thickness 3.17 mm,
Temperature -28.9 °C
17.7 ft-lb

@Thickness 0.125 in,
Temperature -20.0 °F
Geometry GC; ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
ASTM D648