Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 1180 MPa | 171000 psi | 0.5 in/min; ASTM D790B |
ExxonMobil PP7414 Polypropylene Homopolymer Product Description: A medium impact strength copolymer resin designed for injection-molded automotive applications requiring medium melt flow rate.Availability: North America Features:Impact Modif.. |
|||
Flexural Modulus, 1% Secant | 1180 MPa | 171000 psi | ASTM-D790 |
Braskem AC59 HDPE Monofilament Polyethylene Homopolymer AC59 resin is a high-density polyethylene homopolymer produced by the solution process and designed for monofilament applications. It contains antioxidant additives. Its applications include: film .. |