Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 1030 MPa | 150000 psi | ASTM D790B |
ExxonMobil HDPE HD 8760.29 High Density Polyethylene Resin Product Description: HD 8760 is a high density hexene copolymer designed to offer outstanding stiffness and processability. This resin is ideally suited for applications that require the optimum bal.. |
|||
Flexural Modulus, 1% Secant | 1030 MPa | 150000 psi | ASTM D790B |
ExxonMobil HDPE HD P8760.29 High Density Polyethylene Resin Product Description: HD 8760 is a high density hexene copolymer designed to offer outstanding stiffness and processability. This resin is ideally suited for applications that require the optimum bal.. |
|||
Flexural Modulus, 1% Secant | 1030 MPa | 150000 psi | 0.05 in/min; ASTM D790A |
ExxonMobil PP7414 Polypropylene Homopolymer Product Description: A medium impact strength copolymer resin designed for injection-molded automotive applications requiring medium melt flow rate.Availability: North America Features:Impact Modif.. |
|||
Flexural Modulus, 1% Secant | 1030 MPa | 149000 psi | ASTM D790A |
Dow C7014-35RNA Polypropylene Impact Copolymer Resin DOW™ C7014-35RNA Polypropylene Resin is a high impact copolymer intended for injection molding processes. It is especially suited for thin-wall flow path molds.Main CharacteristicsFast set-upEasy .. |
|||
Flexural Modulus, 1% Secant | 1030 MPa | 149000 psi | ASTM D790A |
Dow C702-20 Polypropylene Impact Copolymer Resin OverviewHigh impactComplies with: U.S. FDA FCN 843, Canadian HPFB No ObjectionDOW C702-20 Polypropylene Resin is intended for use in injection molded applications requiring high impact. It is parti.. |
|||
Flexural Modulus, 1% Secant | 1030 MPa | 149000 psi | ASTM-D790 |
Braskem BS600 HDPE Blow Molding Polyethylene Copolymer BS600 resin is a high-density polyethylene (HDPE), bimodal copolymer offering an outstanding combination of impact resistance and environmental stress crack resistance (ESCR). It is thus recommended.. |