Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 22.2 MPa | 3220 psi | ISO R527 |
Dow INSPIRE™ D7000 Thermoplastic Polyolefin
(discontinued **) Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010, although this grade had previously been removed from Dow's standard product line. |
|||
Tensile Strength, Yield | 22.2 MPa | 3220 psi | 2.0 in/min; ASTM D638 |
ExxonMobil PP7414 Polypropylene Homopolymer Product Description: A medium impact strength copolymer resin designed for injection-molded automotive applications requiring medium melt flow rate.Availability: North America Features:Impact Modif.. |
|||
Tensile Strength, Yield | 22.2 MPa | 3220 psi | 2.0 in/min; ASTM D638 |
ExxonMobil PP7654KNE2 Polypropylene Homopolymer Product Description: A high impact copolymer resin with medium melt flow rate and excellent processing attributes. It is designed for injection molded large consumer and industrial parts.Availabili.. |