Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil LD 201.48 Extrusion Coating for Milk Carton Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Extrusion Grade
Manufacturer Exxon Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LD 201.48 Extrusion Coating for Milk Carton Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: LD 201.48 is an LDPE extrusion coating grade, designed to have excellent processability combined with heat sealability and adhesion. It offers – Excellent neck-in/draw down balance, resulting in low edge trim i.e. less waste and high processing line speed. – Good barrier to water vapor, e.g. for applications in portion packaging (sugar, salt)Availability: Latin America, North America and South America Additive: Antiblock: NoSlip: No Thermal Stabilizer: NoApplications: Coextrusion CoatingExtrusion CoatingExtrusion LaminationFoamsFood packagingIndustrial PackagingLiquid Packaging Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.921 g/cc
0.0333 lb/in³
ExxonMobil Method
Melt Flow 4.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Neck In 3.80 cm
1.50 in
328 ft/min (100 m/min), Constant output at 35 rpm; ExxonMobil Method
4.10 cm
1.61 in
164 ft/min (50 m/min), Constant output at 35 rpm; ExxonMobil Method
Drawdown 3.30 m/s
650 ft/min
Constant output at 35 rpm; ExxonMobil Method
Thermal Properties Metric English Comments
Melting Point 109 °C
228 °F
Peak Melting Temperature; ExxonMobil Method
Vicat Softening Point 95.0 °C
203 °F
ASTM D1525