Physical Properties | Metric | English | Comments |
---|---|---|---|
Neck In | 4.10 cm | 1.61 in | at 1000 ft/min; Neck-in reported is the total of both sides; NOVA Chemicals test method |
NOVA Chemicals Novapol® LC-0517-A LDPE Extrusion Resin Excellent adhesion, High drawdown, Excellent sealabilityApplications: Dry soup pouches, Powdered drink pouches, Pharmaceutical packaging, Potato chip bags, Flexible and snack food packagingAdditives.. |
|||
Neck In | 4.10 cm | 1.61 in | 164 ft/min (50 m/min), Constant output at 35 rpm; ExxonMobil Method |
ExxonMobil LD 201.48 Extrusion Coating for Milk Carton Resin Product Description: LD 201.48 is an LDPE extrusion coating grade, designed to have excellent processability combined with heat sealability and adhesion. It offers – Excellent neck-in/draw down bal.. |
|||
Neck In | 4.10 cm | 1.61 in | 164 ft/min (50 m/min), Constant output at 35 rpm; ExxonMobil Method |
ExxonMobil LD 202.48 Extrusion Coating Resin Product Description: LD 202.48 is an LDPE coating grade, especially designed for high speed, lightweight extrusion coating applications providing: -high speed processability – good heat sealing pro.. |
|||
Neck In | 4.10 cm | 1.61 in | at 100 m/min, 35 rpm, 295°C; ExxonMobil Method |
ExxonMobil LD 206.48 Extrusion Coating Resin
(discontinued **) LD 206.48 is a extrusion coating grade, having good organoleptic properties compared to existing standard low odor/off-taste LDPE extrusion coating polymers.Information provided by ExxonMobil Chemic.. |