Physical Properties Metric English Comments
Drawdown 3.30 m/s
650 ft/min
Constant output at 35 rpm; ExxonMobil Method
ExxonMobil LD 201.48 Extrusion Coating for Milk Carton Resin
Product Description: LD 201.48 is an LDPE extrusion coating grade, designed to have excellent processability combined with heat sealability and adhesion. It offers – Excellent neck-in/draw down bal..