Material Notes:
Product Description: Escorene Ultra UL 7760 is a high viscosity, 26.7% VA copolymer that has very good flexibility and low temperature toughness. It has good compatibility with both hydrocarbon and natural tackifiers and most waxes, and is suitable for making hot melt adhesives, sealants and wax blends.Availability: Latin America, North America and South America Additive: Antiblock: NoSlip: NoThermal Stabilizer: Yes Applications:Adhesives and SealantsIndustrial SealantsHot Melt AdhesivesWax BlendsBonding AdhesivesInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.954 g/cc
0.0345 lb/in³
ExxonMobil method
Vinyl Acetate Content 26.7 %
26.7 %
ExxonMobil method
Melt Flow 5.7 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.7 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 76

@Time 15.0 sec
76

@Time 0.00417 hour
ASTM D2240
Hardness, Shore D 27

@Time 15.0 sec
27

@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 8.27 MPa
1200 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Flexural Modulus, 1% Secant 28.3 MPa
4100 psi
ASTM D790
Thermal Properties Metric English Comments
Melting Point <= 163 °C
<= 325 °F
Peak Melting Point; ExxonMobil method
Vicat Softening Point 46.1 °C
115 °F
ASTM D1525