Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 8.27 MPa | 1200 psi | 510 mm/min; ASTM D412A |
PolyOne Elastamax™ XL-2085 Thermoplastic Polyolefin Elastomer (TPO (POE)) PolyOne's Elastamax™ XL thermoplastic olefins (TPOs) are based on pelletized blends of polyolefin resins and select elastomers such EPDM. These materials have been engineered to provide a balance o.. |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible C6502 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex Monprene® MP 7002 Thermoplastic Elastomer Notes: Semi-transparent Features: Good Chemical and Oil ResistanceInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex Monprene® MP-1579D Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex Monprene® MP-1580D Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex Monprene® MP-1846-L3 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex Monprene® MP 1580L1 Thermoplastic Elastomer Notes: USP Class VI; Translucent Features: High Throughput Uses: Medical TubingInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex Monprene® MP-2676 UV Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex Monprene® MP-2840M Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex Monprene® MP-2850E Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex Telcar® TL EF-6155 UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex Telcar® TL-1536D Thermoplastic Elastomer Uses: Consumer Applications; General Purpose; Household Goods; Food Containers; Handles; Lids Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat.. |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex Telcar® TL-1654D Thermoplastic Elastomer Notes: Non-halogenated; RoHS Compliant; MBDC: Green Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General .. |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | 20 in/min; ASTM D412 |
Teknor Apex Telcar® TL-86-K875-F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | ASTM D638 |
Teknor Apex Vidux® CV-92-A5008A-91 Polyvinyl Chloride, Flexible Notes: RoHS Compliant Features: Antistatic; Conductive; Electromagnetic Shielding (EMI); Non-DEHP Plasticizer; Ethylene Oxide Sterilizable; Radio Frequency Shielding (RFI) Uses: Coating Applications.. |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | 500 mm/min (20 in./min); ASTM-D638 Type IV Specimen |
Westlake EMAC® SP2409 20% EMA Copolymer Westlake EMAC� SP2409 is a 20% EMA copolymer designed for extrusion coating, tie-layers, and extrusions where flexibility, compatibility, low heat seal temperatures, or a high coefficient of fr.. |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex Telcar® TL-97-T0214B-55 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex Uniprene® UN-7100-80 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | ASTM D638 |
ExxonMobil HDPE HD 6704.18 High Density Polyethylene Copolymer Resin Product Description: HD 6704 is a narrow molecular weight hexane copolymer designed for outstanding balance of ESCR, Toughness and Stiffness properties. This resin is ideally suited for heavy-duty a.. |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | ISO 527-2/1A/50 |
ExxonMobil LDPE LD 650 Low Density Polyethylene Resin (European Grade) Product Description: LD 650 is an easy flowing LDPE grade with a good flexibility and excellent toughness.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: NoSlip: No.. |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | ASTM D638 |
ExxonMobil Optema® TC-110 Molding Ethylene Methyl Acrylate Product Description: Optema TC 110 is an ethylene methyl acrylate copolymer. TC 110 can be used for injection molding applications. It can be used in alloys, blends or compounds to increase impact s.. |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | ASTM D638 |
Entec Hypel® PELD20/.920 LDPE Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 121-80B230 Thermoplastic Elastomer A soft, black thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is specially formulated to bond to sulfur or peroxide-cured thermoset EPDM rubber for corner .. |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | Molded and tested in accordance with ASTM D4976; ASTM D638 |
Dow DNDA-9810 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-9810 NT 7 is produced using UNIPOL™ PE process technology and is supplied in pellet form. This resin is specifically designed as a carrier resin for color concentrates and other masterbat.. |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | Molded and tested in accordance with ASTM D4976; ASTM D638 |
Dow FLEXOMER™ GERS-1088 NT Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ GERS-1088 NT is an ethylene-butene copolymer produced via gas phase polymerization from Dow. It can be utilized in monolayer and co-extruded films and in blends with other polyolefins to.. |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex Monprene® MP 1245A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | Across Flow; ASTM D412 |
ExxonMobil Geolast® 701-80W183 Thermoplastic Elastomer A soft, black, oil resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good hot air and hot oil resistance for use in a wide range of applic.. |