Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Schott BG24A Band Pass Filter

Category Ceramic , Glass , Optical , Filter
Manufacturer Schott Glas Mainz
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schott BG24A Band Pass Filter.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.
Physical Properties Metric English Comments
Density 2.72 g/cc
0.0983 lb/in³
Thermal Properties Metric English Comments
CTE, linear 8.50 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.72 µin/in-°F

@Temperature -22.0 - 158 °F
9.70 µm/m-°C

@Temperature 20.0 - 300 °C
5.39 µin/in-°F

@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 460 °C
860 °F
Optical Properties Metric English Comments
Refractive Index 1.52

@Wavelength 1014 nm
1.52

@Wavelength 1014 nm
Hg
1.53

@Wavelength 587.6 nm
1.53

@Wavelength 587.6 nm
He
1.55

@Wavelength 365 nm
1.55

@Wavelength 365 nm
Hg
1.59

@Wavelength 253.7 nm
1.59

@Wavelength 253.7 nm
Hg
Transmission, Visible <= 1.0 %

@Wavelength 560 - 630 nm
<= 1.0 %

@Wavelength 560 - 630 nm
89 %

@Wavelength 400 nm
89 %

@Wavelength 400 nm
Internal transmittance of 97% at 400 nm
IR Transmittance 89 %

@Wavelength 730 - 750 nm
89 %

@Wavelength 730 - 750 nm
Internal transmittance of 97% from 730-740 nm.
UV Transmittance <= 20 %

@Wavelength 200 - 210 nm
<= 20 %

@Wavelength 200 - 210 nm
91 %

@Wavelength 320 - 380 nm
91 %

@Wavelength 320 - 380 nm
Internal transmittance of 99% from 320-370 nm
Reflection Coefficient, Visible (0-1) 0.92
0.92
Chemical Properties Metric English Comments
Acid Class, SR 3
3
Alkali Class, AR 2
2
Stain Resistance Class, FR 0.0
0.0
Copyright © lookpolymers.com All Rights Reserved