Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 150 g/10 min @Load 2.16 kg, Temperature 190 °C |
150 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil EXXELOR™ PO 1015 Maleic anhydride functionalized polypropylene Product Description: Exxelor Po 1015 polymer resin is a maleic anhydride fuctionalized polypropylene copolymer, produced by reactive extrusion. It has been primarily designed to add polarity to poly.. |