HEMA phthalate, also known as MEP or PAMM, Phthalic Acid Monoethyl Methacrylate is an aromatic, carboxylic acid-containing monomer lends itself to many adhesive and emulsion applications where the functionality of a methacrylate is needed. One common application is anaerobic adhesives. Listed on the Toxic Substance Control Act List. CAS # 27697-00-3.Information provided by ESSTECH, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
Viscosity 5000 cP

@Temperature 25.0 °C
5000 cP

@Temperature 77.0 °F
Molecular Weight 278.26 g/mol
278.26 g/mol
Optical Properties Metric English Comments
Refractive Index 1.526
1.526
Processing Properties Metric English Comments
Moisture Content <= 0.50 %
<= 0.50 %
Descriptive Properties Value Comments
Color (APHA) < 400
HEMA Purity (%) < 20
MeHQ Inhibitor (ppm) 100
MEP Purity (%) > 75