Solvay DURAPHOS® 524 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name DURAPHOS®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay DURAPHOS® 524 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Identification: TRIARYL PHOSPHATES, ISOPROPYLATEDCAS: 68937-41-7; 115-86-6 Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: DURAPHOS® 524 is an ashless, antiwear and mild extreme pressure additive for lubricants and metal working formulations.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.131 - 1.141 g/cc
0.04086 - 0.04122 lb/in³
ISO12185
Chemical Properties Metric English Comments
Total Acid Number <= 0.10
<= 0.10
ISO6618
Processing Properties Metric English Comments
Moisture Content <= 0.10 %
<= 0.10 %
ISO-760
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Clear Liquid, No Visible Contamination
Color <75
APHA or HAZEN, ISO2211
Composition Free Phenols
<0.05
Phosphorous Content
7.3-7.8