Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total PPH M3382MZ Homopolymer Polypropylene, Clarified Metallocene Sheet Extrusion and Thermoforming Resin

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Sheet/Thermoforming Grade
Manufacturer Total Atofina
Trade Name PPH
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PPH M3382MZ Homopolymer Polypropylene, Clarified Metallocene Sheet Extrusion and Thermoforming Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Clarity. TOTAL Polypropylene M3382MZ produces thermoformed parts with superior clarity, gloss and excellent side wall stiffness.Recommended Applications. TOTAL Polypropylene M3382MZ is ideal for deli containers, drinking cups, lids, domes and food service trays when high clarity and stiffness are important.High Purity. TOTAL Polypropylene M3382MZ features minimum extractables and optimum thermal stability for superior color and processability.FDA. TOTAL Polypropylene M3382MZ complies with all applicable FDA regulations and may be used under these provisions for food contact and packaging.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.905 g/cc
0.905 g/cc
ISO 1183
Melt Flow 3.2 g/10 min
3.2 g/10 min
ASTM D1238, L
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.0 MPa
4500 psi
ASTM D638
Elongation at Yield >= 65 %
>= 65 %
ASTM D638
Flexural Modulus 1.49 GPa
216 ksi
ASTM D790
Izod Impact, Notched 0.587 J/cm
1.10 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Melting Point 153 °C
307 °F
DSC
Deflection Temperature at 0.46 MPa (66 psi) 97.0 °C
207 °F
ASTM D648